Magnesium Alloy ZK60A

  • Magnesium Alloy ZK60A
  • General Characteristics

    The ZK60A is used where high strength and good toughness are required. This alloy is heat treatable and is normal used in the artificially aged (T5) condition. Alloy ZK60A has essentially the same strength as AZ80A but with greater ductility. To develop maximum properties, both AZ80A and ZK60A are heat treated to the artificially aged (T5) condition; AZ80A may be given the T6 solution heat treatment, followed by artificial aging to provide maximum creep stability. Typical uses include extruded products and press forgings with high strength and good ductility.

  • Typical Chemical Composition

    Weight % Zn Zr Other (total) Mg
    minimum 4.80 0.45 Bal
    maximum 6.20 0.30
  • Physical Properties

    Characteristics English Metric
    Nominal density 25°C   /   78°F 0.066 lbs/in3 1.83 g/cm3
    Specific heat Cp=0.1233+0.0002566T+3939T2
    Incipient melting >=965 °F >=518 °C
    Coefficient of thermal

    expansion

    20°C   /   68°F 14 micro in/in- °F 26 micro m/m- °K
    Thermal conductivity F temper

    20°C (68°F)

    68 BTU/ft- hr – °F 117 W/m – °K
    T5 temper

    20°C (68°F)

    70 BTU/ft- hr – °F 121 W/m – °K
    Electrical conductivity F temper

    20°C (68°F)

    29 %IACS
    T5 temper

    20°C (68°F)

    30 %IACS
  • Mechanical Properties

    Condition Tensile Hardness Shear strength
    Ultimate Yield Elongation in

    50 mm

    (2 in.)

    Brinell

    500 kg load,

    10 mm ball

    KSI MPa KSI MPa % KSI Mpa
    F temper 49 340 38 260 11 75 27 185
    T5 temper 51 350 41 285 11 82 26 180
  • Specifications

    • AMS – 4352, QQ-M-31B
    • ASTM – B107